Stainless Steel: Mechanism and Classification


 

The basic principle is that the element Cr (chromium) forms a Cr2O3 passivation layer on contact with the oxygen in the air.

The passivation layer protects the base metal from other corrosive substances it comes into contact with.

Other elements that contribute to passivation are Ni, Mo and Ti (nickel, molybdenum, titanium). Although there are more than 200 stainless steel grades in total, only 10% of them are widely used in applications.

Stainless steels, which can deliver strikingly attractive results especially in aesthetic terms, are available in forms such as coil, plate/sheet, wire, bar, hexagon bar, flat bar and angle.

Microstructure in particular is of great importance to today's metallurgists / metallurgical and materials engineers for project design, process design and material design.

In addition to their excellent corrosion resistance, stainless steels are available in grades with varying mechanical properties. Their properties are modified by adding or removing elements such as carbon (C), nickel (Ni), molybdenum (Mo), sulfur (S), titanium (Ti), copper (Cu), vanadium (V), niobium (Nb), nitrogen (N), tungsten (W) and manganese (Mn).

Chromium (Cr) is the key element that gives stainless steels their corrosion resistance. It is a ferrite-stabilizing metal; therefore, plain Fe-Cr alloys have a fully ferritic microstructure at room temperature up to 20% Cr. When chromium (Cr) exceeds 20% Cr, the sigma phase appears. Chromium (Cr) is a strong carbide former. 

Carbon (C) is an austenite-stabilizing element. By increasing the yield strength and tensile strength, it gives stainless steel hardness and strength. 

Nickel (Ni) is an austenite-stabilizing element. When nickel (Ni) reaches 8%, the austenite field expands considerably and the microstructure remains austenitic. It greatly increases resistance to corrosion and oxidation. It increases strength and impact resistance at high or low temperatures. 

Silicon (Si) increases oxidation resistance, is always added to heat-resistant grades, and is a ferrite-stabilizing element.

Aluminum (Al) is also used in heat-resistant alloys and enhances the effect of silicon (Si).

Molybdenum (Mo) strengthens the passivity of stainless steel in acidic and chloride-containing environments and increases its corrosion resistance. 

Tungsten (W) is a ferrite stabilizer and carbide former. It is added to the alloy to improve the mechanical properties of the material. 

Titanium (Ti) and Niobium (Nb) form very stable carbides and are added to austenitic stainless steels to prevent sensitization.

Manganese (Mn), like nickel (Ni), is an austenite-stabilizing element. It increases the strength and durability of stainless steel. In some grades it replaces nickel (Ni) when the nickel content is reduced to lower costs.

Nitrogen (N) is essentially an austenite-stabilizing element, and its effect is similar to that of carbon (C). In some austenitic stainless steels it replaces nickel (Ni) when the nickel content is reduced to lower costs.

Copper (Cu) is a weak austenite stabilizer. It is added to the composition of austenitic stainless steels to increase corrosion resistance in certain environments.

Sulfur (S) is added to improve the machinability of stainless steels. However, it reduces corrosion resistance and weldability.

 


Stainless steels are classified according to their microstructure.


1. Austenitic Stainless Steels
They account for 60% of the world's stainless steel production. They contain a maximum of 0.15% C (carbon), a minimum of 16% Cr (chromium), and sufficient amounts of Ni and Mn (nickel and manganese) to stabilize the austenitic phase structure. The best-known grade is AISI 304.

Owing to their phase structure, they are non-magnetic. They cannot be hardened by heat treatment.

They exhibit high ductility and can be hardened by rolling (cold working). Their corrosion resistance is excellent, and they are machinable and weldable.

They have an FCC (Face Centered Cubic) structure.

It is not possible to draw sharp boundaries in terms of their fields of application. They are used everywhere from the consumer durables sector, such as white goods, to the petrochemical industry.

Super-austenitic stainless steels, on the other hand, are very costly because of their highly alloyed composition.

Austenitic: AISI 303 (1.4305), AISI 304 (1.4301), AISI 304L (1.4307), AISI 316 (1.4401), AISI 316L (1.4404), AISI 316Ti (1.4571), AISI 321 (1.4541), AISI 310/310S (1.4845), AISI 316LMo (1.4435)

Super Austenitic: AISI 904L (1.4439)

 

2. Ferritic Stainless Steels
Ferritic stainless steels are a group of stainless steels that generally contain no Ni (nickel) but have a high chromium content (between 10.5% and 30%), together with alloying elements such as molybdenum, titanium and vanadium that form carbides and stabilize the ferritic structure.

The generally high chromium content gives ferritic stainless steels very high corrosion resistance. Ferritic stainless steels, whose mechanical and physical properties are closer to those of their close relatives, the carbon steels, are magnetic, unlike austenitic grades; because of their low carbon content they cannot be hardened by heat treatment, and they can be rolled easily.

The only heat treatment that can be applied to these steels is annealing. The recent sharp rise and volatility in the prices of alloying elements, especially nickel, has accelerated the development of ferritic grades, and new ferritic grades have been developed that offer corrosion resistance comparable to austenitic grades at low cost, have a wide range of applications and are much cheaper.

The most widely known ferritic grades are 430 and 442.

The structure of ferritic grades is BCC. (Body-Centered Cubic)

The microstructures of a) grade 409 and b) grade 439 ferritic stainless steels are shown below.

3. Martensitic Stainless Steels
With a structure similar to that of ferritic steels, martensitic stainless steels resemble low-alloy – high-strength steels or carbon steels. However, because of their additional carbon content, they can be hardened and strengthened by heat treatment, like carbon steels. Their main alloying elements are 12% to 15% chromium, 0.2% to 1.0% molybdenum and 0.1% to 1.2% carbon. Apart from a few martensitic grades, they contain no nickel. Martensitic stainless steels, an example of whose microstructure is shown above, are magnetic. As the carbon content increases, their hardenability and strength increase while their toughness and ductility decrease. Depending on the high carbon content and other alloying elements, they can be hardened by heat treatment up to 60 HRC. Optimum corrosion resistance is achieved after the stress-relieving heat treatment known as tempering. Compared with ferritic and austenitic grades, the corrosion resistance of martensitic grades is somewhat lower. Their machinability and formability are high. Depending on the alloying elements they contain and their proportions, their structure may contain a small amount of retained austenite. Martensitic steels can be used very successfully especially where strength and resistance to mechanical wear are required together with corrosion resistance. They are also used as tool steels. Their field of application is very wide.


4. Duplex Stainless Steels
Duplex stainless steels are called “duplex” because they have a two-phase microstructure consisting of ferritic and austenitic stainless steel grains. When duplex stainless steel is melted, it solidifies from the liquid phase into a fully ferritic structure. As the material cools to room temperature, about half of the ferritic grains transform into austenitic grains. As a result, duplex stainless steel has a microstructure of roughly 50% austenite and 50% ferrite.
 

5. Precipitation-Hardened Stainless Steels

Precipitation-hardening stainless steels  are a group within the family of Fe-Cr-Ni stainless steels that contain alloying elements such as copper, molybdenum, niobium, titanium and aluminum, and exhibit precipitation hardening through the effect of one or more of these elements.
In principle, precipitation hardening is an aging treatment that follows rapid cooling after solution annealing of the alloy. The alloying elements mentioned above, present in the steel, dissolve during solution annealing and, during aging, precipitate as very fine particles, increasing the hardness and strength of the matrix. As a result of this treatment, the steel can attain the mechanical properties of martensitic stainless steels and the corrosion resistance of 304-series austenitic stainless steels. The most important advantage of these steels in production is that, after being easily machined and formed in the normalized condition, their mechanical properties are improved by a heat treatment at 480-600°C. Their strength can reach approximately 1700 MPa, thus exceeding the strength of martensitic stainless steels.

Precipitation-hardening stainless steels are classified into three types according to the structural changes and properties of the steel resulting from the treatments after solution annealing. These are martensitic precipitation-hardening stainless steels, semi-austenitic precipitation-hardening stainless steels and austenitic precipitation-hardening stainless steels.

 Precipitation-hardening stainless steels produced today are widely used in the outer skins of high-speed aircraft, missile bodies, marine vessels, fuel tanks, aircraft landing gear, pumps, shafts, nuts, bolts, cutting tools and clutches (Tülbentçi et al., 1993).